Alloy | Density lb./in3 (g/cm3) |
Sheet, Plate & Strip |
Billet Rod/Bar |
Coated Electrodes |
Bare Welding Rods |
Seamless Pipe & Tube |
Welded Pipe & Tube |
Fittings | Forgings | DIN | Other |
HAYNES® 25 alloy R30605 |
0.330 (9.13) |
AMS 5537 | AMS 5759 MIL-C-24252D |
AMS 5797 | AMS 5796 | – | – | – | AMS 5759 | – | MIL-R-5031B Class 13 |
HAYNES® 188 alloy R30188 |
0.324 (8.98) |
AMS 5608 | AMS 5772 | – | – | – | – | – | AMS 5772 | – | – |
HAYNES® 230® alloy N06230 HAYNES® 230-W® alloy N06231 |
0.324 (8.97) |
AMS 5878 SB 435/B 435 P=43 |
AMS 5891 SB 572/B 572 B 472 P=43 |
SFA 5.11/ A 5.11 (ENiCrWMo-1) F= 43 |
SFA 5.14/ A 5.14 (ERNiCrWMo-1) AMS 5839 F= 43 |
SB 622/B 622 P=43 |
SB 619/B 619 SB 626/B 626 P=43 |
SB 366/B 366 P=43 |
AMS 5891 SB 564/B 564 P=43 |
17744 No. 2.4733 NiCr22W14Mo |
– |
HAYNES® 242® alloy N10242 |
0.327 (9.05) |
SB 434/B 434 P=44 |
SB 573/B 573 B 472 P= 44 |
– | SFA 5.14 A 5.14 (ERNiMo-12) F= 44 |
SB 622/B 622 P=44 |
SB 619/B 619 SB 626/B 626 P=44 |
SB 366/B 366 P=44 |
SB 564/B 564 P=44 |
– | – |
HAYNES® 263 alloy N07263 |
0.302 (8.36) |
AMS 5872 | AMS 5886 | – | AMS 5966 | – | – | – | AMS 5886 | – | – |
HAYNES® 282® alloy N07208 |
AMS 5951 | B 637 AMS 5951 |
– | – | – | – | – | B 637 AMS 5951 |
– | – | |
HAYNES® 556® alloy R30556 |
0.297 (8.22) |
AMS 5874 SB 435/B 435 P=45 |
AMS 5877 SB 572/B 572 B 472 P= 45 |
– | SFA 5.9/ A 5.9 (ER3556) AMS 5831 F= 6 |
SB 622/B 622 P=45 |
SB 619/B 619 SB 626/B 626 P=45 |
SB 366/B 366 P=45 |
AMS 5877 | No. 1.4883 X10CrNiCoMoN 22 20 18 |
– |
HAYNES® 617 alloy N06617 (W86117) |
0.302 (8.36) |
AMS 5888 AMS 5889 SB 168/B 168 P=43 |
SB 166/B 166 B 472 AMS 5887 P=43 |
SFA 5.11/ A 5.11 (ENiCrCoMo-1) F= 43 |
SFA 5.14/ A 5.14 (ERNiCrCoMo-1) F= 43 |
SB 167/B 167 P=43 |
– | – | SB 564/B 564 P=43 |
– | – |
HAYNES® 625 alloy N06625 (W86112) |
0.305 (8.44) |
AMS 5599 SB 443/B 443 AMS 5869 |
AMS 5666 SB 446/B 446 B 472 P= 43 |
SFA 5.11/ A 5.11 (ENiCoMo-3) F= 43 |
SFA 5.14/ A 5.14 (ERNiCrMo-3) AMS 5837 F= 43 |
AMS 5581 SB 444/B 444 P=43 |
AMS 5581 SB 704/B 704 SB 705/B 705 P=43 |
SB 366/B 366 P=43 |
AMS 5666 SB 564/B 564 P=43 |
17744 No. 2.4856 NiCr22Mo9Nb |
AMSE Code Case No. 2468 NACE MR0175 ISO 15156 |
HAYNES® 625SQ® alloy N06626 |
0.305 (8.44) |
AMS 587 ASME Code Case 2276 |
– | – | – | – | ASME Code Case No. 2276 P=43 |
ASME Code Case No. 2276 P=43 |
– | – | – |
HAYNES® 718 alloy N07718 |
0.297 (8.22) |
AMS 5596 AMS 5597 |
AMS 5662 AMS 5663 AMS 5664 SB 637/B 637 |
– | A 5.14 (ERNiFeCr-2) AMS 5832 |
AMS 5589 AMS 5590 B 983 |
– | – | AMS 5662 AMS 5663 AMS 5664 SB 637/B 637 |
17742 No. 2.4668 NiCr19Fe19NbMo3 |
ASME Code Case No. 1993-6 Case No. 2221-1 NACE MR0175 ISO 15156 |
HAYNES® HR-120® alloy N08120 |
0.291 (8.05) |
AMS 5916 SB 409/B 409 P=45 |
SB 408/B 408 B 472 P=45 |
– | – | SB 407/B 407 SB 163/B 163 P=45 |
SB 514/B 514 SB 515/B 515 P=45 |
SB 366/B 366 P=45 |
SB 564/B 564 P=45 |
No. 2.4854 NiFe33Cr25Co |
|
HAYNES® HR-160® alloy N12160 |
0.292 (8.08) |
SB 435/B 435 P=46 |
SB 572/B 572 P=46 |
– | SFA 5.14/ A 5.14 (ERNiCoCrSi-1) F= 46 |
SB 622/B 622 P= 46 |
SB 619/B 619 SB 626/B 626 P=46 |
SB 366/B 366 P=46 |
SB 564/B 564 P=46 |
No. 2.4880 NiCo29Cr28Si |
ASME Code Case No. 2385 |
MULTIMET® R30155 (W73155) |
0.296 (8.19) |
AMS 5532 | AMS 5678 | AMS 5794 SFA 5.4/ A 5.4 (E3155) |
AMS 5794 | – | – | – | AMS 5768 AMS 5769 B 639 |
– | – |
HAYNES® R-41 alloy N07041 |
0.298 (8.25) |
AMS 5545 | AMS 5712 | – | AMS 5800 | – | – | – | AMS 5712 | – | – |
HAYNES® Waspaloy alloy N07001 |
0.296 (8.19) |
AMS 5544 | AMS 5704 AMS 5706 AMS 5707 SB 637/B 637 |
– | AMS 5828 | – | – | – | AMS 5704 AMS 5706 AMS 5707 SB 637/B 637 |
– | – |
HASTELLOY® X alloy N06002 (W86002) |
0.297 (8.22) |
AMS 5536 SB 435/B 435 P=43 |
AMS 5754 SB 572/B 572 B 472 P=43 |
SFA 5.11/ A 5.11 (ENiCrMo-2) F= 43 |
SFA 5.14/ A 5.14 (ERNiCrMo-2) AMS 5798 F= 43 |
SB 622/B 622 P= 43 |
AMS 5588 SB 619/B 619 SB 626/B 626 P=43 |
SB 366/B 366 P=43 |
AMS 5754 | 17742 Mo. 2.4665 NiCr22Fe18Mo |
NACE MR0175 ISO 15156 |
HAYNES® X-750 alloy N07750 |
0.298 (8.25) |
AMS 5542 AMS 5598 |
AMS 5667 AMS 5668 AMS 5670 AMS 5671 AMS 5747 |
– | SFA 5.1/ A 5.14 (ERNiCrFe-8) AMS 5778 |
– | – | – | AMS 5667 AMS 5668 AMS 5670 AMS 5671 AMS 5747 SB 637/B 637 |
No. 2.4669 NiCr15Fe7TiAl |
NACE MR0175 ISO 15156 |