Tubular products sizes for
HAYNES® and HASTELLOY® alloys
- Seamless: 1/2” to 4-1/2”
- Seamless Titanium: 1/4” to 1-1/2”
- Welded: 1/2” to 8” Sch. 40
Seamless Pipe and Tubing
Seamless pipe and tubing is covered under the appropriate specifications. Cold-worked seamless pipe and tubing is produced from billets by either trepanning or extrusion followed by pilgering and/or drawing.
HAYNES® Ti-3Al-2.5V alloy
Ti-3Al-2.5V alloy was developed for aircraft hydraulicand fuel systems transmission lines, primarily because of its high strength-to-weight ratio. Thisratio proved to be a major design advantage when used for hydraulic tubing lines, providing required strength levels, but more importantly, reducing weight by as much as 43% when compared to stainless steel.
Welded Pipe
Welded pipe is formed, welded, solution heat-treated, and tested in accordance with appropriate specifications.
Welded Tubing
Welded tubing is made from strip by forming, welding, sizing or cold-working, solution heat treating, and testing in accordance with the applicable specifications. The classes of welded tubing available are as follows:
- as welded and solution-annealed
- welded and fully cold-reduced or welded and bead-worked
Bead-worked vs. welded and fully cold-reduced
Fully cold-reduced tubing is the cold reduction of both the weld seam and base metal (parent material.) The minimum reduction is generally 20% of the total area and achieves optimum metallurgical conditions. Bead worked tubing is the cold reduction of the weld seam only, generally reducing the weld seam only by 2-10%.
Photomicrographs of Weld Bead
Magnified at 200x
Bead Worked
Fully Cold-reduced
The Tubular Products Manufacturing Facility. , established in 1976 and located in Arcadia, Louisiana, produces welded and seamless pipe and tubing. The Tubular facility has more than 36 years’ experience in producing HASTELLOY®, HAYNES® alloys and Titanium 3Al-2.5V tubular products.
Our 200,000 square foot tubular facility houses a complete range of pilgering, welding and drawing equipment designed especially for the manufacture of diverse sizes of seamless and welded products in HAYNES®, HASTELLOY®, and titanium Ti-3AL-2.5V alloys.
The tubular uses feedstock produced from the Kokomo, Indiana mill to fabricate welded and seamless alloy pipe and tubing and purchases extruded tube hollows to produce seamless titanium tubing. Manufacturing processes at Arcadia require cold pilger mills, weld mills, draw benches, annealing furnaces and pickling facilities.
Our Manufacturing Equipment
- 9 Pilger mills
- 1 Draw bench
- 2 Continuous weld mills
- 1 Pipe mill
- 3 Vacuum furnaces
- 1 Continuous roller hearth furnace
- 5 UT testers for inspection
Quality
Our products exceed the most rigorous specifications and are trusted worldwide to provide exacting service requirements. We use state-of the art inspection equipment and methods to provide process control and ensure product integrity. Samples are tested for conformance to the chemical composition requirements of the applicable specification.
Consistent quality levels with optimum metallurgical conditions are sought by plant personnel when using welded tubular products. In theory, procurement to ASTM specifications should lead to assurance of consistent, well-defined metallurgical conditions. However, the ASTM specifications leave the option to the buyer to select between the cold working of the weld-metal only (bead working) or of cold working both the weld and the base metal (cold-reduction via drawing or pilgering). As such, additional detailed specifications are required to insure optimum metallurgical conditions for best resistance to corrosion.
Inspection and Nondestructive Testing
- NDT Testing
- UT Testers
- Eddy-current
- Hydrostatic
- Pneumatic
- Liquid-penetrant
- Visual (white glove test)
- Dimensional
Visual Inspection (White Glove Test)
Destructive Lab Testing
- Tensile
- Hydrostatic
- Flare
- Flange
- Flats
- Metallographic analysis
- Corrosion
- Gas analysis
- CSR Testing
- Bends
PED:
Accredited Welding Processes
Accredited Welding Operators
We are the premier choice in innovative solutions for demanding applications. Our welded and seamless high-performance alloy tubulars are manufactured to the exacting requirements of aerospace, gas turbine, chemical processing, power pollution control, oil and gas, refining, agricultural, pulp and paper, marine, and many other industries.
Corrosion-resistant alloys
Specifications | Available Forms | ||||||
---|---|---|---|---|---|---|---|
Alloy | UNS | Seamless Pipe & Tubing |
Welded Pipe & Tubing |
Tubing | Pipe | ||
Welded | Seamless | Welded | Seamless | ||||
B-3® | N10675 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
C-4 | N06455 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
C-22® | N06022 | SB 622/ B 622 | SB 619/B 619 SB 626/B 626 |
||||
C-22HS® | N07022 | B 983 | – | ||||
C-276® | N10276 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
C-2000® | N06200 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
G-30® | N06030 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
G-35® | N06035 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
HYBRID-BC1® | N10362 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
Available from stock in select sizes
Available with approval and minimum quantities Oil country tubulars
High-temperature alloys
Specifications | Available Forms | ||||||
---|---|---|---|---|---|---|---|
Alloy | UNS | Seamless Pipe & Tubing |
Welded Pipe & Tubing |
Tubing | Pipe | ||
Welded | Seamless | Welded | Seamless | ||||
25 | R30605 | – | – | – | – | ||
188 | R30188 | – | – | – | – | ||
214® | N07214 | – | – | – | – | ||
230® | N06230 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
242® | N10242 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
263 | N07263 | – | – | – | – | – | – |
282® | N07208 | – | – | – | |||
556® | R30556 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
– | – | ||
617 | N06617 | SB 167/B 167 | – | – | – | – | – |
625 | N06625 | AMS 5581 SB 444/B 444 |
AMS 5581 SB 704/ B 704 SB 705/B 705 |
||||
625SQ® | N06626 | – | ASME Code Case No. 2276 |
||||
718 | N07718 | AMS 5589 AMS 5590 B 983 |
– | ||||
HR-120® | N08120 | SB 407/B 407 SB 163/B 163 |
SB 514/B 514 SB 515/B 515 |
||||
HR-160® | N12160 | SB 622/B 622 | SB 619/B 619 SB 626/B 626 |
||||
HR-235® | N06235 | ASTM B167 | ASTM B619 ASTM B626 |
||||
X | N06002 | SB 622/B 622 | AMS 5588 SB 619/B 619 SB 626/B 626 |
– | – | ||
X-750 | N07750 | AMS 5582 AMS 5583 |
– | – | – |
Available from stock in select sizesAvailable with approval and minimum Quantities Oil country tubulars
Titanium alloy
Specifications | Available Forms | ||||||
---|---|---|---|---|---|---|---|
Alloy | UNS | Seamless Pipe & Tubing |
Welded Pipe & Tubing |
Tubing | Pipe | ||
Welded | Seamless | Welded | Seamless | ||||
Ti-3Al-2.5V | R5632 | AMS 4943 AMS 4944 AMS 4945 AMS 4946 AS5620 SB 338/ B 338Gr9 |
– | – | – | – |
Available from stock in select sizes Available with approval and minimum QuantitiesOil country tubulars