Barra lista para uso final, Barra que requiere procesamiento adicional
Hot-Rolled Bar
Standard Sizes:
- Diameter: 0.312”- 3.5″ (7.925- 88.9 mm)
- Length: up to 12 feet (3.66 m)
Standard Finishes:
- Annealed and Centerless Ground
- Annealed and Pickled
Forged Bar
Standard Sizes:
- Diameter: 3.75”- 9″ (95 mm – 228 mm)
- Length: up to 12 feet (3.66 m)
Standard Finishes:
- Annealed, Turned and Ground
- Annealed and Pickled
- Annealed and Turned
Round Billet
Standard Sizes:
- Diameter: 3.75”- 14″ (95 mm – 355 mm)
- Length: up to 12 feet (3.66 m)
Standard Finishes:
- As-forged and Turned
- As-forged, Turned, and Polished
- As-forged and Ground
Round-Cornered Squares Billet
Standard Sizes:
- Diameter: 3.75”- 14″ (95 mm – 355 mm)
- Length: up to 12 feet (3.66 m)
Standard Finishes:
- As-forged and Ground
Ingot
Standard Sizes:
- Diameter up to 26” (660 mm)