HASTELLOY® C-2000® Coated Electrodes

Home / Product Forms / Wire and Welding / Coated Electrodes / HASTELLOY® C-2000® Coated Electrodes

Product Description:

HASTELLOY® C-2000® coated electrodes are used for the shielded metal arc welding of C-2000® alloy. The deposited weld metal has excellent resistance to uniform corrosion conditions in a variety of media including oxidizing and reducing environments. The alloy makes a great candidate for dissimilar joining of other nickel-chromium-molybdenum alloys and also molybdenum containing stainless steels. The electrodes are also used for the overlay and cladding of carbon steels where enhanced corrosion resistance is needed.

Specifications:

AWS A 5.11 ENiCrMo-17   Kennblatt 9677.03
ASME Code Case 2334     UNS W86200
*Specify at time of order

Composition:

Nickel Balance
Chromium 22.0-24.0
Molybdenum 15.0-17.0
Iron 3.0 max.
Cobalt 2.0 max.
Copper 1.3-1.9
Manganese 0.50 max.
Other 0.50 max.
Silicon 0.20 max.
Carbon 0.02 max.
Phosphorus 0.03 max.
Sulfur 0.015 max.

Minimum Mechanical Properties:

Tensile (psi) 100,000
Mpa 690
Elongation (%) 25

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150