Titanium alloy
Specifications | Available Forms | ||||||
---|---|---|---|---|---|---|---|
Alloy | UNS | Seamless Pipe & Tubing |
Welded Pipe & Tubing |
Tubing | Pipe | ||
Welded | Seamless | Welded | Seamless | ||||
Ti-3Al-2.5V | R5632 | AMS 4943 AMS 4944 AMS 4945 AMS 4946 AS5620 SB 338/ B 338Gr9 |
– | – | – | – |
Available from stock in select sizes Available with approval and minimum QuantitiesOil country tubulars