Specifications for Corrosion-resistant Alloys

Home / Specifications for Corrosion-resistant Alloys
Alloy
Densitylb./in3 (g/cm3)
Sheet, Plate & Strip BilletRod/Bar Coated Electrodes Bare Welding Rods Seamless Pipe & Tube Welded Pipe & Tube Fittings Forgings DIN TUV Other
HASTELLOY®  B-3® alloy N10675 (W80675) 0.333(9.22) SB-333/B333 P=44

SB-335/ B335
B 472
P=44

SFA 5.11/ A 5.11(ENiMo-10)
DIN 2.4696
(EL-NiMo28Cr)
F= 44

SFA 5.14/ A 5.14
(ERNiMo-10)
DIN 2.4695
(SG-NiMo30Cr)
F=44

SB-622/B622 P=44 SB-619/B619 SB-626/B626 P=44 SB-366/B366 SB-462/B462 P=44 SB-564/B564 SB-462/B 462 P=44 17744 No. 2.4600 NiMo29Cr Werkstoffblatt 517 Kennblatt 7615 Kennblatt 7616 Kennblatt 7617 –
HASTELLOY® C-4 alloyN06455 (W86455) 0.312(8.64) SB-575/B575 P=43 SB-574/B574 P=43
SFA 5.11/ A 5.11(ENiCRMo-7)
DIN 2.4612
(EL-NiMo15Cr15Ti)
F= 43
SFA 5.14/ A 5.14(ERNiCrMo-7)
DIN 2.4611
(SG-NiMo16Cr16Ti) F= 43
SB-622/B622 P=43 SB-619/B619 SB-626/B626 P=43 SB 366/B366 P=43 - 17744 No. 2.4610 NiMo16Cr16Ti Werkstoffblatt 424 Kennblatt 2666 Kennblatt 2667 Kennblatt 2665 NACE MR0175 ISO 15156
HASTELLOY® C-22® alloy N06022 (W86022) 0.314(8.69) SB-575/B575 P=43 SB-574/B574 B472 P=43
SFA 5.11/ A 5.11(ENiCrMo-10)
DIN 2.4638
(EL-NiCr21Mo14W) F= 43
SFA 5.14/ A 5.14(ERNiCrMo-10)
DIN 2.4635
(SG-NiCr21Mo14W) F= 43
SB-622/B622 P=43 SB-619/B619 SB-626/B626 P=43 SB-366/B366 SB-462/B462 P=43 SB-564/B564 SB-462/B462 P=43 17744 No. 2.4602 NiCr21Mo14W Werkstoffblatt 479 Kennblatt 4635 Kennblatt 4536 Kennblatt 4534 NACE MR0175 ISO 15156 ASME Code Case No. 2226-2Case No. N-621-1
HASTELLOY®C-22HS® alloy N07022 0.311(8.61) – B 637 – – B 983 – – B 637 – – NACE MR0175
HASTELLOY® C-276 alloy N10276 (W10276) 0.321(8.89) SB-575/B575 P=43 SB-574/B574 B472 P=43
SFA-5.11/ A5.11(ENiCrMo-4)
DIN 2.4887
(EL-NiMo15Cr15W)
F= 43
SFA 5.14/ A 5.14(ERNiCrMo-4)
DIN 2.4886
(SG-NiMo16Cr16W)
F= 43
SB-622/B622 B983
P=43
SB-619/B619 SB-626/B626 P=43 SB-366/B366 SB-462/B462 P=43 SB-564/B564 SB-462/B462 P=43 17744 No. 2.4819 NiMo16Cr15W Werkstoffblatt 400 Kennblatt 320 Kennblatt 319 NACE MR0175 ISO 15156
HASTELLOY®C-2000® alloy N06200 (W86200) 0.307(8.50) SB-575/B575 P=43 SB-574/B574 B472 P=43
SFA 5.11 (ENiCrMo-17) A5.11(ENiCrMo-17)
DIN 2.4699 (EL-NiCr23Mo16Cu)
F= 43
SFA 5.14/ A 5.14(ERNiCrMo-17)
DIN 2.4698(SG-NiCr23Mo16Cu) F= 43
SB-622/B622 P=43 SB-619/B619 SB-626/B626 P=43 SB-366/B366 SB-462/B462 P=43 SB-564/B564 SB-462/B462 P=43 17744 No. 2.4675NiCr23Mo16Cu Werkstoffblatt 539 Kennblatt 9679 Kennblatt 9678 Kennblatt 9677 NACE MR0175 ISO 15156
HASTELLOY®  G-30® alloy N06030 (W86030) 0.297(8.22) SB-582/B582
P=45
SB-581/B581 B472
P=45
SFA 5.11/ A 5.11
(ENiCrMo-11)
F= 45
SFA 5.14/ A 5.14(ERNiCrMo-11)
F= 45
SB-622/B622 P=45 SB 619/B619 SB 626/B 626 P=45 SB 366/B366 SB 462/B 462 P=45 SB 462/B 462 P=45 No. 2.4603 NiCr30FeMo – NACE MR0175 ISO 15156
HASTELLOY® G-35® alloy N06035 0.297(8.22) SB-575/B575
P=43
SB-574/B574 B472
P=43
SFA 5.11/ A 5.11
(ENiCrMo-22)
F=43
SFA 5.14/ A 5.14
(ERNiCrMo-22)
F=43
SB-622/B622 P=43 SB 619/B619 SB 626/B 626 P=43 SB 366/B366 SB 462/B 462 P=43 SB 564/B564 SB 462/B 462 P=43 No. 2.4643 NiCr33Mo8 – NACE MR0175 ISO 15156 ASME Code Case No. 2484
HASTELLOY®  HYBRID-BC1® alloy N10362 0.319(8.83) B575 P=43 B574 B472 P=43 SFA 5.11/A5.11 (ENiMoCr-1) F=43 ASME Code Case No. 2653 SFA 5.14/A5.14 (ENiMoCr-1) F=44 B622 P=43 B 619 B 626 P=43 B 366 P=43 B 462B 564 P=43 No. 2.4708 NiMo22Cr15 – NACE MR0175 ISO 15156
HASTELLOY® N alloy N10003 0.320(8.86) AMS 5607 SB-434/B434 P=44 AMS 5771 SB-573/B573 P=44 –
SFA 5.14/ A 5.14 (ERNiCrMo-2)
F= 44
– – SB 366/B366 P=44 AMS 5771 – – Mil-N24390B
ULTIMET® alloy R31233 0.306(8.47) SB-818/B818 SB-815/B815 – SFA / A5.21 (ERCoCr-H) – – – – No. 2.4681 CoCr26Ni9Mo5W – NACE MR0175/MR0103 ISO 15156