HASTELLOY® B-3® Coated Electrodes

Home / Product Forms / Wire and Welding / Coated Electrodes / HASTELLOY® B-3® Coated Electrodes

Product Description:

HASTELLOY® B-3® coated electrodes are used for the shielded metal arc welding of B-3® alloy materials. The weld metal has excellent resistance to hydrochloric acids at all temperatures and also withstands hydrogen chloride, sulfuric, acetic and hydrofluoric acids. The alloy has improved thermal stability and resistance to stress corrosion cracking over alloy B-2. The electrode can be used for the overlay and cladding of carbon and stainless steels with no butter layer needed. The coating is developed for great operability, especially in out-of-position welding.

Specifications:

AWS A 5.11 ENiMo-10              ASME IX F-43
ASME SFA 5.11 ENiMo-10       UNS W860675
Kennblatt 7617.02*
*Specify at time of order

Composition:

Nickel Balance
Molybdenum 27.0-32.0
Iron 1.0-3.0
Chromium 1.0-3.0
Cobalt 3.0 max.
Tungsten 3.0 max.
Manganese 2.0 max.
Copper 0.50 max.
Other 0.50 max.
Silicon 0.20 max.
Carbon 0.02 max.
Sulfur 0.03 max.
Phosphorus 0.04 max.

Minimal Mechanical Properties:

Tensile (psi) 100,000
Mpa 690
Elongation (%) 25

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150

Packaged in Hermetically Sealed Containers