Product Description:
HASTELLOY® C-2000® coated electrodes are used for the shielded metal arc welding of C-2000® alloy. The deposited weld metal has excellent resistance to uniform corrosion conditions in a variety of media including oxidizing and reducing environments. The alloy makes a great candidate for dissimilar joining of other nickel-chromium-molybdenum alloys and also molybdenum containing stainless steels. The electrodes are also used for the overlay and cladding of carbon steels where enhanced corrosion resistance is needed.
Specifications:
AWS A 5.11 ENiCrMo-17 Kennblatt 9677.03
ASME Code Case 2334 UNS W86200
*Specify at time of order
Composition:
|
Nickel |
Balance |
|
Chromium |
22.0-24.0 |
|
Molybdenum |
15.0-17.0 |
|
Iron |
3.0 max. |
|
Cobalt |
2.0 max. |
|
Copper |
1.3-1.9 |
|
Manganese |
0.50 max. |
|
Other |
0.50 max. |
|
Silicon |
0.20 max. |
|
Carbon |
0.02 max. |
|
Phosphorus |
0.03 max. |
|
Sulfur |
0.015 max. |
Minimum Mechanical Properties:
|
Tensile (psi) |
100,000 |
|
Mpa |
690 |
|
Elongation (%) |
25 |
Available Product Forms and Sizes:
|
Diameter in |
0.093 |
0.125 |
0.156 |
0.187 |
|
Diameter mm |
2.40 |
3.20 |
4.00 |
4.70 |
|
Length in |
10 |
14 |
14 |
14 |
|
Length mm |
254 |
355.6 |
355.6 |
355.6 |
|
Package Weight lbs. |
5 |
10 |
10 |
10 |
|
Current (A) DCEP |
40-70 |
70-100 |
80-140 |
120-150 |