| Alloy |
Density lb./in3 (g/cm3) |
Sheet,Plate & Strip | Billet Rod/Bar | Coated Electrodes | Bare Welding Rods | Seamless Pipe & Tube | Welded Pipe & Tube | Fittings | Forgings | DIN | Other |
|---|---|---|---|---|---|---|---|---|---|---|---|
| HAYNES® 25 alloy R30605 | 0.327 (9.07) | AMS 5537 | AMS 5759 MIL-C-24252D | AMS 5797 | AMS 5796 | – | – | – | AMS 5759 | – | NACE MR0175 ISO 15156 |
| HAYNES® 188 alloy R30188 | 0.324(8.98) | AMS 5608 | AMS 5772 | – | AMS 5801 | – | – | – | AMS 5772 | – | – |
|
HAYNES® 230® alloy N06230 HAYNES® 230-W® alloy N06231 |
0.324(8.97) | AMAS 5878 SB-435/B435 P=43 | AMS 5891 SB 572/B 572 B 472 P=43 | SFA 5.11/ A 5.11 (ENiCrWMo-1) F= 43 | SFA 5.14/ A 5.14 (ERNiCrWMo-1) AMS 5839 F= 43 | SB-622/B622P=43 | SB-619/B619 SB 626/B626 P=43 | SB 366/B 366 P=43 | AMS 5891 SB-564/B564 P=43 | 17744 No. 2.4733 NiCr22W14Mo | – |
| HAYNES® 242® alloy N10242 | 0.327(9.05) | SB 434/B434 P=44 | SB 573/B 573B 472 P=44 | – | SFA 5.14A 5.14 (ERNiMo-12) F= 44 | SB 622/B 622 P=44 | SB-619/B619 SB 626/B 626 P=44 | SB 366/B 366 P=44 | SB 564/B 564 P=44 | – | – |
| HAYNES® 263 alloy N07263 | 0.302(8.36) | AMS 5872 | AMS 5886 | – | AMS 5966 | – | - | – | AMS 5886 | – | – |
| HAYNES® 282® alloy N07208 | 0.299 (8.27) | AMS 5951 | B 637 AMS 5915 | – | – | – | – | – | B637 AMS 5915 | – | – |
| HAYNES® 556® alloy R30556 | 0.297 (8.23) | AMAS 5874 SB-435/B435 P=45 | AMAS 5877 SB-572/B572 B472 P=45 | – | SFA 5.9 (ER3556) A5.9 (ER3556) AMS 5831 F=6 | SB 622/B 622 P=45 | SB 619/B 619SB 626/B 626 P=45 | SB 366/B 366 P=45 | AMS 5877 | No. 1.4883 X10CrNiCoMoN 22 20 18 | – |
| HAYNES® 617 alloy N06617 (W86117) | 0.302(8.36) | AMS 5888AMS 5889SB 168/B 168 P=43 | SB 166/B 166B 472 AMS 5887 P=43 | SFA 5.11/ A 5.11 (ENiCrCoMo-1) F= 43 | SFA 5.14/ A 5.14(ERNiCrCoMo-1) F= 43 | SB 167/B 167 P=43 | B626 B546 | – | SB 564/B 564 P=43 | – | – |
| HAYNES® 625 alloy N06625 (W86112) | 0.305(8.44) | AMS 5599 SB 443/B 443 AMS 5869 P=43 | AMS 5666 SB 446/B 446 B 472 P=43 | SFA 5.11/ A 5.11(ENiCoMo-3) F= 43 | SFA 5.14/ A 5.14(ERNiCrMo-3)AMS 5837 F= 43 | AMS 5581SB 444/B 444 P=43 | AMS 5581 SB 704/B 704 SB 705/B 705 P=43 | SB 366/B 366 P=43 | AMS 5666 SB-564/B564 P=43 | 17744 No. 2.4856NiCr22Mo9Nb | AMSE CodeCase No. 2468 NACE MR0175 ISO 15156 |
| HAYNES® 625SQ® alloy N06626 | 0.305(8.44) | AMS 5879 ASME Code Case 2276 | – | – | – | – | ASME CodeCase No. 2276 P=43 | ASME Code Case No. 2276 P=43 | – | – | – |
| HAYNES® 718 alloy N07718 | 0.297(8.23) | AMS 5596 AMS 5597 SB 670/B670 | AMS 5662 AMS 5663 AMS 5664 SB 637/B 637 | – | A 5.14 (ERNiFeCr-2) AMS 5832 | AMS 5589 AMS 5590 B983 | – | – | AMS 5662 AMS 5663 AMS 5664 SB-637/B637 | 17742 No. 2.4668NiCr19Fe19NbMo3 | ASME CodeCase No. 1993-6 Case No. 2221-1NACE MR0175 ISO 15156 |
| HAYNES® HR-120® alloy N08120 | 0.291(8.07) | AMS 5916 SB-409/B409 | SB-408/B408 B472 | – | – | SB-407/B407 SB-163/B163 | SB-514/B514 SB-515/B515 | SB-366/B366 P=43 | SB-564/B564 | No. 2.4854NiFe33Cr25Co | |
| HAYNES® HR-160® alloy N12160 | 0.292(8.08) | AMS 5916 SB435/B435 SB435/B435 P=46 | SB-572/B572 B472 P=46 | – | SFA 5.14/ A 5.14(ERNiCoCrSi-1)F= 46 | SB 622/B 622 P=4446 | SB 619/B 619SB 626/B 626 | SB-366/B366 P=46 | SB 564/B564 P=46 | No.2.4880NiCo29Cr28Si | ASME CodeCase No. 2385 |
| HAYNES® HR-235® alloy N06235 | 0.295 (8.16) | B168 / SB-168 | B166 / SB-166 | – | – | ASTM B167 B167 / SB-167 B622 ASTM B622 | ASTMB619 B619 / SB-619 B626 / SB-626 ASTM B626 | ASTM B366 | B366 / SB-366 | – | – |
| MULTIMET® R30155 (W73155) | 0.296(8.20) | AMS 5532 | AMS 5678 | AMS 5795SFA 5.4/ A 5.4 (E3155) | AMS 5794 | – | – | – | AMS 5768 AMS 5769B639 | – | – |
| HAYNES® R-41 alloy N07041 | 0.298(8.25) | AMS 5545 | AMS 5712 | – | AMS 5800 | – | – | – | AMS 5712 | – | – |
| HAYNES® Waspaloy alloy N07001 | 0.296(8.20) | AMS 5544 | AMS 5704AMS 5706AMS 5707SB 637/B 637 | – | AMS 5828 | – | – | – | AMS 5768AMS 5769B639 | – | – |
| HASTELLOY® X alloy N06002 (W86002) | 0.297(8.22) | AMS 5536SB 435/B 435 | AMS 5754SB 572/B 572B 472 | SFA 5.11/ A 5.11(ENiCrMo-2)F= 43 | SFA 5.14/ A 5.14(ERNiCrMo-2)AMS 5798F= 43 | SB 622/B 622 P=43 | AMS 5588 SB-619/B619 SB-626/B626 P=43 | SB 366/B 366 P=43 | AMS 5754 | 17742 Mo. 2.4665NiCr22Fe18Mo | NACE MR0175ISO 15156 |
| HAYNES® X-750 alloy N07750 | 0.298(8.26) | AMS 5542AMS 5598 | AMS 5667AMS 5668AMS 5670AMS 5671AMS 5747 | – | SFA 5.1/ A 5.14(ERNiCrFe-8)AMS 5778 | – | – | – | AMS 5667AMS 5668AMS 5670AMS 5671AMS 5747SB 637/B 637 | No. 2.4669NiCr15Fe7TiAl | NACE MR0175ISO 15156 |