| Alloy |
Densitylb./in3 (g/cm3) |
Sheet, Plate & Strip | BilletRod/Bar | Coated Electrodes | Bare Welding Rods | Seamless Pipe & Tube | Welded Pipe & Tube | Fittings | Forgings | DIN | TUV | Other |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| HASTELLOY® B-3® alloy N10675 (W80675) | 0.333(9.22) | SB-333/B333 P=44 |
SB-335/ B335 |
SFA 5.11/ A 5.11(ENiMo-10) |
SFA 5.14/ A 5.14 |
SB-622/B622 P=44 | SB-619/B619 SB-626/B626 P=44 | SB-366/B366 SB-462/B462 P=44 | SB-564/B564 SB-462/B 462 P=44 | 17744 No. 2.4600 NiMo29Cr | Werkstoffblatt 517 Kennblatt 7615 Kennblatt 7616 Kennblatt 7617 | – |
| HASTELLOY® C-4 alloyN06455 (W86455) | 0.312(8.64) | SB-575/B575 P=43 | SB-574/B574 P=43 |
SFA 5.11/ A 5.11(ENiCRMo-7)DIN 2.4612 (EL-NiMo15Cr15Ti) F= 43 |
SFA 5.14/ A 5.14(ERNiCrMo-7) DIN 2.4611 (SG-NiMo16Cr16Ti) F= 43 |
SB-622/B622 P=43 | SB-619/B619 SB-626/B626 P=43 | SB 366/B366 P=43 | - | 17744 No. 2.4610 NiMo16Cr16Ti | Werkstoffblatt 424 Kennblatt 2666 Kennblatt 2667 Kennblatt 2665 | NACE MR0175 ISO 15156 |
| HASTELLOY® C-22® alloy N06022 (W86022) | 0.314(8.69) | SB-575/B575 P=43 | SB-574/B574 B472 P=43 |
SFA 5.11/ A 5.11(ENiCrMo-10) DIN 2.4638 (EL-NiCr21Mo14W) F= 43 |
SFA 5.14/ A 5.14(ERNiCrMo-10) DIN 2.4635 (SG-NiCr21Mo14W) F= 43 |
SB-622/B622 P=43 | SB-619/B619 SB-626/B626 P=43 | SB-366/B366 SB-462/B462 P=43 | SB-564/B564 SB-462/B462 P=43 | 17744 No. 2.4602 NiCr21Mo14W | Werkstoffblatt 479 Kennblatt 4635 Kennblatt 4536 Kennblatt 4534 | NACE MR0175 ISO 15156 ASME Code Case No. 2226-2Case No. N-621-1 |
| HASTELLOY®C-22HS® alloy N07022 | 0.311(8.61) | – | B 637 | – | – | B 983 | – | – | B 637 | – | – | NACE MR0175 |
| HASTELLOY® C-276 alloy N10276 (W10276) | 0.321(8.89) | SB-575/B575 P=43 | SB-574/B574 B472 P=43 |
SFA-5.11/ A5.11(ENiCrMo-4) DIN 2.4887 (EL-NiMo15Cr15W) F= 43 |
SFA 5.14/ A 5.14(ERNiCrMo-4)DIN 2.4886 (SG-NiMo16Cr16W) F= 43 |
SB-622/B622 B983 P=43 | SB-619/B619 SB-626/B626 P=43 | SB-366/B366 SB-462/B462 P=43 | SB-564/B564 SB-462/B462 P=43 | 17744 No. 2.4819 NiMo16Cr15W | Werkstoffblatt 400 Kennblatt 320 Kennblatt 319 | NACE MR0175 ISO 15156 |
| HASTELLOY®C-2000® alloy N06200 (W86200) | 0.307(8.50) | SB-575/B575 P=43 | SB-574/B574 B472 P=43 |
SFA 5.11 (ENiCrMo-17) A5.11(ENiCrMo-17) DIN 2.4699 (EL-NiCr23Mo16Cu) F= 43 |
SFA 5.14/ A 5.14(ERNiCrMo-17)DIN 2.4698(SG-NiCr23Mo16Cu) F= 43 |
SB-622/B622 P=43 | SB-619/B619 SB-626/B626 P=43 | SB-366/B366 SB-462/B462 P=43 | SB-564/B564 SB-462/B462 P=43 | 17744 No. 2.4675NiCr23Mo16Cu | Werkstoffblatt 539 Kennblatt 9679 Kennblatt 9678 Kennblatt 9677 | NACE MR0175 ISO 15156 |
| HASTELLOY® G-30® alloy N06030 (W86030) | 0.297(8.22) | SB-582/B582 P=45 | SB-581/B581 B472 P=45 |
SFA 5.11/ A 5.11(ENiCrMo-11) F= 45 |
SFA 5.14/ A 5.14(ERNiCrMo-11) F= 45 |
SB-622/B622 P=45 | SB 619/B619 SB 626/B 626 P=45 | SB 366/B366 SB 462/B 462 P=45 | SB 462/B 462 P=45 | No. 2.4603 NiCr30FeMo | – | NACE MR0175 ISO 15156 |
| HASTELLOY® G-35® alloy N06035 | 0.297(8.22) | SB-575/B575 P=43 | SB-574/B574 B472 P=43 |
SFA 5.11/ A 5.11(ENiCrMo-22) F=43 |
SFA 5.14/ A 5.14 (ERNiCrMo-22) F=43 |
SB-622/B622 P=43 | SB 619/B619 SB 626/B 626 P=43 | SB 366/B366 SB 462/B 462 P=43 | SB 564/B564 SB 462/B 462 P=43 | No. 2.4643 NiCr33Mo8 | – | NACE MR0175 ISO 15156 ASME Code Case No. 2484 |
| HASTELLOY® HYBRID-BC1® alloy N10362 | 0.319(8.83) | B575 P=43 | B574 B472 P=43 | SFA 5.11/A5.11 (ENiMoCr-1) F=43 | ASME Code Case No. 2653 SFA 5.14/A5.14 (ENiMoCr-1) F=44 | B622 P=43 | B 619 B 626 P=43 | B 366 P=43 | B 462B 564 P=43 | No. 2.4708 NiMo22Cr15 | – | NACE MR0175 ISO 15156 |
| HASTELLOY® N alloy N10003 | 0.320(8.86) | AMS 5607 SB-434/B434 P=44 | AMS 5771 SB-573/B573 P=44 | – |
SFA 5.14/ A 5.14 (ERNiCrMo-2) F= 44 |
– | – | SB 366/B366 P=44 | AMS 5771 | – | – | Mil-N24390B |
| ULTIMET® alloy R31233 | 0.306(8.47) | SB-818/B818 | SB-815/B815 | – | SFA / A5.21 (ERCoCr-H) | – | – | – | – | No. 2.4681 CoCr26Ni9Mo5W | – | NACE MR0175/MR0103 ISO 15156 |