MULTIMET® Coated Electrodes

Home / Product Forms / Wire and Welding / Coated Electrodes / MULTIMET® Coated Electrodes

Product Description:

MULTIMET® coated electrodes are used for the shielded metal arc welding of HAYNES® HR-120® alloy. The electrodes are also a great candidate for dissimilar joining of other high-temperature materials including HAYNES® 556® alloy, HAYNES® HR-160® alloy and other nickel and cobalt high-temperature alloys. The coating is designed for great operability, especially in out-of-position welding.

Specifications:

AMS 5795

Composition:

Iron Remainder
Chromium 20.0-22.5
Nickel 19.0-21.0
Cobalt 18.5-21.0
Molybdenum 2.5-3.5
Tungsten 2.0-3.0
Manganese 1.0-2.5
Niobium + Tantalum 0.75-1.25
Silicon 1.0 max.
Carbon 0.10 max.
Phosphorus 0.04 max.
Sulfur 0.03 max.

Minimal Mechanical Properties:

Tensile (psi) 90,000
Mpa 620
Elongation (%) 20

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150