Product Description:
HAYNES® HR-160® RTW™ filler metal is used for the gas metal arc and gas tungsten arc welding of HAYNES® HR-160® alloy. The alloy has outstanding resistance to high-temperature corrosion, including sulfidation and chloride attack in reducing and oxidizing atmospheres. The alloy also is a great candidate for thermal spray applications where resistance to high-temperature abrasion and corrosion are required. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.
Specifications:
AWS A5.14 ERNiCoCrSi-1 UNS N12160
Composition:
| Nickel | Remainder |
| Cobalt | 27.0-32.0 |
| Chromium | 26.0-29.0 |
| Iron | 3.5 max. |
| Silicon | 2.4-3.0 |
| Manganese | 1.0 max. |
| Molybdenum | 0.70 max. |
| Titanium | 0.20-0.60 |
| Copper | 0.50 max. |
| Tungsten | 0.50 max. |
| Other | 0.30 max. |
| Aluminum | 0.40 max. |
| Niobium + Tantalum | 0.15 max. |
| Carbon | 0.02-0.10 |
| Sulfur | 0.02 max. |
| Phosphorus | 0.03 max. |
Minimal Mechanical Properties
| Tensile (psi) | 90,000 |
| Mpa | 620 |
| Elongation (%) | 60 |
Available Product Forms and Sizes:
| Diameter in | 0.030 | 0.031 | 0.035 | 0.039 | 0.045 | 0.047 | 0.062 | 0.078 | 0.093 | *0.125 | *0.156x | 0.187x |
| Diameter mm | 0.76 | 0.80 | 0.89 | 1.00 | 1.10 | 1.20 | 1.60 | 2.00 | 2.40 | *3.20 | *4.00x | *4.70x |
Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.
*Size not available in MIG spools.
˟Size not available on reels.
Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.