HASTELLOY® G-35® RTW™ Filler Metal

Product Description:

HASTELLOY® G-35® RTW™ filler metal is used for the gas metal and gas tungsten arc welding of G-35® alloy. The weld metal has outstanding corrosion resistance to “fertilizer-grade” phosphoric acid, other oxidizing acids, alkalis, and chloride-bearing media. The RTW™ finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AWS A5.14 ERNiCrMo-22    UNS N06035

Composition:

Nickel Balance
Chromium 32.25-34.25
Iron 2.00 max.
Molybdenum 7.60-9.00
Cobalt 1.00 max.
Tungsten 0.60 max.
Titanium 0.20 max.
Vanadium 0.20 max.
Manganese 0.30 max.
Silicon 0.50 max.
Other 0.60 max.
Phosphorus 0.03 max.
Carbon 0.05 max.
Sulfur 0.015 max.
Aluminum 0.40 max.
Niobium + Tantalum 0.50 max.

Minimal Mechanical Properties:

Tensile (psi) 85,000
Mpa 590
Elongation (%) -

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.