Product Description:
HASTELLOY® C-22® RTW™ filler metal is used for the gas metal and gas tungsten arc welding of HASTELLOY® C-22®alloy. The deposited weld metal has low thermal expansion characteristics, good oxidation resistance to 1500°F (815°C) and excellent fabricability. The alloy is used in gas turbine seal rings, containment structures and high-strength fasteners. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.
Specifications:
AWS A5.14 ERNiCrMo-10 UNS N06022
ASME-SFA-5.14 ERNiCrMo-10 ASME IX F-43
Kennblatt 4536.05(C/L)* Kennblatt 4535.04 (Spools)*
ASME-SFA-5.14 ERNiCrMo-10
*Specify at time of order
Composition:
| Nickel | Balance |
| Chromium | 20.0-22.5 |
| Molybdenum | 12.5-14.5 |
| Iron | 2.0-6.0 |
| Tungsten | 2.5-3.5 |
| Cobalt | 2.5 max. |
| Manganese | 0.50 max. |
| Other | 0.50 max. |
| Copper | 0.50 max. |
| Vanadium | 0.35 max. |
| Silicon | 0.08 max. |
| Phosphorus | 0.02 max. |
| Carbon | 0.015 max. |
| Sulfur | 0.010 max. |
Minimal Mechanical Properties:
| Tensile (psi) | 115,000 |
| Mpa | 793 |
| Elongation (%) | 40 |
Available Product Forms and Sizes:
| Diameter in | 0.030 | 0.031 | 0.035 | 0.039 | 0.045 | 0.047 | 0.062 | 0.078 | 0.093 | *0.125 | *0.156x | 0.187x |
| Diameter mm | 0.76 | 0.80 | 0.89 | 1.00 | 1.10 | 1.20 | 1.60 | 2.00 | 2.40 | *3.20 | *4.00x | *4.70x |
Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.
*Size not available in MIG spools.
˟Size not available on reels.
Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.