HASTELLOY® 622 RTW™ Filler Metal

Product Description:

HASTELLOY® 622 RTW™ filler metal is used for weld overlay applications and has an enriched chemistry for outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. It has excellent resistance to oxidizing aqueous media including wet chlorine. The weld metal has excellent resistance to preferential corrosive attack in various media and thus is a great candidate for overlay and cladding of carbon steels. The alloy makes a great candidate for dissimilar welding of other nickel-chromium-molybdenum alloys and stainless steels. The RTW™ finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AWS A5.14 ERNiCrMo-10           UNS N06022
ASME-SFA-5.14 ERNiCrMo-10

Composition:

Nickel Balance
Chromium 22.1-22.5
Molybdenum 14.0-14.5
Tungsten 3.25-3.5
Cobalt 2.50 max.
Copper 0.50 max.
Manganese 0.50 max.
Other 0.50 max.
Vanadium 0.35 max.
Silicon 0.08 max.
Phosphorus 0.02 max.
Carbon 0.015 max.
Sulfur 0.010 max.

Minimal Mechanical Properties:

Tensile Strength (psi) 115,000
Tensile Strength (MPa) 793
Elongation (%) 40

Available Product Forms and Sizes:

Diameter, in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x *0.187x
Diameter, mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths.

Other lengths available upon request.