Product Description:
A cobalt-based, solid wire, ULTIMET®wire is used to weld ULTIMET® wrought products, and more importantly, to overlay and clad carbon and low-alloy steels. The weld deposits harden very quickly by cold working. In addition, it is very easy to deposit a “crack-free” layer without a butter layer. The RTW™ filler metal finish on the MIG-spooled wire promotes smooth feeding through welding equipment and reduce tip wear in contact tips.
Key Features:
- ULTIMET®wire easily produces crack-free weld deposits (over-matching weld overlays, weld inlays, and claddings).
- It is easier to weld with ULTIMET® wire than traditional cobalt-based alloys, allowing multiple layer build-ups with no pre-heating needed.
- ULTIMET® wire produces deposits which harden quickly through peening, machining, power hammering, burnishing, or hard particle impingement. This hardness creates a tough, ductile, wear-, corrosion-, and high-temperature resistant surface. The hardness of 30% cold-worked wrought product is approximately RC 50.
- ULTIMET®deposits exhibit extremely high resistance to metal to metal galling and seizing.
- The pitting resistance of ULTIMET®alloy in chloride solutions is equal to that of HASTELLOY®C-22HS®alloy, and is greater than that of C-276 alloy.
Applications:
- Valve component overlay
- “Make/break” seal welds in threaded unions
- Weld overlays to marine riser tensioners, shafts, and larger hydraulic system pistons
- Weld overlay to u-bends, piping and vales used in conveying sour crudes containing abrasives
- Slurry, rock, and acid tumblers and mixers
- Impellers
- Fiberglas manufacturing
Composition:
| Cobalt | Balance |
| Chromium | 23.5-27.5 |
| Nickel | 7.0-11.0 |
| Molybdenum | 4.0-6.0 |
| Iron | 1.0-5.0 |
| Tungsten | 1.0-3.0 |
| Manganese | 0.10-1.5 |
| Silicon | 0.05-1.0 |
| Nitrogen | 0.03-0.12 |
| Carbon | 0.02-0.10 |
| Phosphorus | 0.030 max. |
| Sulfur | 0.020 max. |
| Boron | 0.015 max. |
Specifications:
| UNS R31233 | - |
| DIN CoCr26Ni9Mo5W | - |
| DIN No. 2.4681 | - |
Minimal Mechanical Properties:
| Tensile (psi) | 133,000 |
| Mpa | 917 |
| Elongation (%) | 10 |
Available Product Forms and Sizes:
| Diameter in | 0.030 | 0.031 | 0.035 | 0.039 | 0.045 | 0.047 | 0.062 | 0.078 | 0.093 | *0.125 | *0.156x | *0.187x |
| Diameter mm | 0.76 | 0.80 | 0.89 | 1.00 | 1.10 | 1.20 | 1.60 | 2.00 | 2.40 | *3.20 | *4.00x | *4.70x |
Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.
*Size not available in MIG spools.
˟Size not available on reels.
Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.