Product Description:
HAYNES® 117 coated electrodes are used for the shielded metal arc welding of HAYNES® 617 alloy. The weld metal has excellent high-temperature strength and resistance to oxidation. The 117 alloy electrodes are also useful for making dissimilar welds between other high-temperature materials such as 600, 601 and 800. The coating is designed for great operability, especially out-of-position welding.
Specifications:
AWS A 5.11 ENiCrCoMo-1 ASME IX F-43
ASME SFA 5.11 ENiCrCoMo-1 UNS W86117
Composition:
|
Nickel |
Balance |
|
Chromium |
21.0-26.0 |
|
Cobalt |
9.0-15.0 |
|
Molybdenum |
8.0-10.0 |
|
Iron |
5.0 max. |
|
Manganese |
0.3-2.5 |
|
Niobium + Tantalum |
1.0 max. |
|
Silicon |
0.75 max. |
|
Copper |
0.5 max. |
|
Other |
0.5 max. |
|
Carbon |
0.05-0.15 |
|
Phosphorus |
0.03 max. |
|
Sulfur |
0.015 max. |
Minimum Mechanical Properties:
|
Tensile (psi) |
90,000 |
|
Mpa |
620 |
|
Elongation (%) |
30 |
Available Product Forms and Sizes:
|
Diameter in |
0.093 |
0.125 |
0.156 |
0.187 |
|
Diameter mm |
2.40 |
3.20 |
4.00 |
4.70 |
|
Length in |
10 |
14 |
14 |
14 |
|
Length mm |
254 |
355.6 |
355.6 |
355.6 |
|
Package Weight lbs. |
5 |
10 |
10 |
10 |
|
Current (A) DCEP |
40-70 |
70-100 |
80-140 |
120-150 |