HAYNES®112 coated electrodes are used for the shielded metal arc welding of 625, 825 and molybdenum-containing alloys. The weld metal has good resistance to corrosion including pitting and crevice corrosion. In addition, the electrodes are useful for overlay and cladding of various grades of steel including stainless, low alloy and carbon steels. The electrode makes a great dissimilar joining electrode when joining HAYNES® and HASTELLOY® materials to stainless and carbon steels. The coating is designed for great operability, especially out-of-position welding.
Specifications:
AWS A 5.11 ENiCrMo-3 ASME IX F-43 ASME SFA 5.11 ENiCrMo-3 UNS W86112