HAYNES® 82 RTW™ Filler Metal

Product Description:

HAYNES®82 RTW™ filler metal wire is used for gas metal arc, gas tungsten arc and submerged arc welding of alloy 600, 601, 800 and 825. The alloy can also be used in dissimilar welding applications with carbon and stainless steels, HAYNES® and HASTELLOY® alloys and nickel-copper alloys. The weld metal has good corrosion and oxidation resistance. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AWS A5.14 ERNiCr-3           UNS N06082
ASME-SFA-5.14 ERNiCr-3   ASME IX F-43

Composition:

Nickel 67.0 min.
Chromium 18.0-22.0
Manganese 2.5-3.5
Iron 3.0 max
Niobium 2.0-3.0
Tantalum 0.30 max.
Titanium 0.75 max.
Silicon 0.50 max.
Copper 0.50 max
Other 0.50 max
Carbon 0.10 max.
Phosphorus 0.03 max.
Sulfur 0.03 max.
Cobalt 0.12 max.*

Minimal Mechanical Properties:

Tensile (psi) 80,000
Mpa 552
Elongation (%) 30

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.