HAYNES® 556® RTW™ Filler Metal

Product Description:

HAYNES® 556RTW™ filler metal is used for the gas metal arc and gas tungsten arc welding of HAYNES® HR-120® alloy to itself. The alloy is also a great candidate for dissimilar welding of other high-temperature alloys including HR-160®alloy and other nickel and cobalt high-temperature materials. The weld metal has excellent resistance to high-temperature corrosive environments including WTE, heart-treating, refinery and boiler applications. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AMS 5831                UNS R30566
AWS A5.9 ER3556

Composition:

IronRemainder
Chromium21.0-23.0
Nickel19.0-22.5
Cobalt16.0-21.0
Molybdenum2.5-4.0
Tungsten2.0-3.5
Manganese0.50-2.0
Tantalum0.30-1.25
Silicon0.80 max.
Aluminum0.50 max.
Nitrogen0.30 max.
Niobium0.30 max.
Carbon0.15 max.
Zirconium0.15 max.
Lanthanum0.10 max.
Phosphorus0.04 max.
Boron0.02 max.
Sulfur0.015 max.

Minimal Mechanical Properties

Tensile (psi)107,300
Mpa740
Elongation (%)43.1

Available Product Forms and Sizes:

Diameter in0.0300.0310.0350.0390.0450.0470.0620.0780.093*0.125*0.156x0.187x
Diameter mm0.760.800.891.001.101.201.602.002.40*3.20*4.00x*4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.