HAYNES® 25 RTW™ Filler Metal

Product Description:

HAYNES®25 RTW™ filler metal is used for the gas metal arc and gas tungsten arc welding of HAYNES®25 alloy. The deposited weld metal has excellent strength, good oxidation resistance to 1800°F (980°C), very good sulfidation resistance, and relatively good resistance to wear and galling. The RTW™ finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AMS 5796     UNS R30605

Composition:

Cobalt Remainder
Chromium 19.0-21.0
Tungsten 14.0-16.0
Nickel 9.0-11.0
Iron 3.0 max.
Manganese 1.0-2.0
Silicon 1.0 max.
Carbon 0.05-0.15
Phosphorus 0.04 max.
Sulfur 0.03 max.

Minimal Mechanical Properties:

Tensile (psi) 140,000
Mpa 965
Elongation (%) 40

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.