HAYNES® 242® RTW™ Filler Metal

Product Description:

HAYNES® 242®RTW™ filler metal is used for the gas tungsten arc and gas metal arc welding of HAYNES® 242®alloy. The deposited weld metal has low thermal expansion characteristics, good oxidation resistance to 1500°F (815°C) and excellent fabricability. The alloy is used in gas turbine seal rings, containment structures and high-strength fasteners. The RTW™ finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AWS A5.14 ERNiMo-12   UNS N10242

Composition:

Nickel Remainder
Molybdenum 24.0-26.0
Chromium 7.0-9.0
Iron 2.0 max.
Cobalt 1.0 max.
Manganese 0.80 max.
Silicon 0.80 max.
Aluminum 0.50 max.
Copper 0.50 max.
Carbon 0.03 max.
Phosphorous 0.030 max.
Sulfur 0.015 max.

Minimal Mechanical Properties

Tensile (psi) 100,000
Mpa 690
Elongation (%) -

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.