HAYNES® 214® RTW™ Filler Metal (Structural)

Home / Product Forms / Wire and Welding / TIG (GTAW) and MIG (GMAW) Filler Metal Products / HAYNES® 214® RTW™ Filler Metal (Structural)

Product Description:

HAYNES® 214®RTW™ filler metal is used for the gas metal arc and gas tungsten arc welding of HAYNES® 214®alloy. The deposited weld metal has outstanding oxidation resistance to 2300°F and excellent resistance to carburization and excellent resistance to chlorine-bearing environments. The alloy is used in demanding industrial heating applications and specialized gas turbine parts, such as honeycomb seals. The RTW™ finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

HAYNES PS-6076-2    UNS N07214

Composition:

Nickel Balance
Chromium 15.00-17.00
Aluminum 4.10-5.00
Iron 2.00-4.00
Cobalt 2.00 max.
Manganese 0.50 max.
Molybdenum 0.50 max.
Titanium 0.50 max.
Tungsten 0.50 max.
Silicon 0.20 max.
Niobium 0.15 max.
Carbon 0.05 max.
Yttrium 0.003-0.04
Zirconium 0.02 max.
Phosphorus 0.015 max.
Sulfur 0.015 max.
Magnesium 0.010 max.
Boron 0.004 max.

Minimal Mechanical Properties:

Tensile (psi) –
Mpa –
Elongation (%) –

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.

Footer