HASTELLOY® C-4 RTW™ Filler Metal

Product Description:

HASTELLOY® C-4RTW™ filler metal is used for the gas metal and gas tungsten arc welding of C-4alloy. The deposited weld metal has outstanding high-temperature stability in the 1200°F to 1900°F range. The weld metal has excellent resistance to stress corrosion cracking and oxidizing atmospheres up to 1900°F. It also resists a wide variety of chemical process environments. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AWS A5.14 ERNiCrMo-7     UNS N06455
ASME SFA-5.14 ERNiCrMo-7

Composition:

Nickel Remainder
Chromium 14.0-18.0
Molybdenum 14.0-18.0
Iron 3.0 max.
Cobalt 2.0 max.
Manganese 1.0 max.
Titanium 0.70 max.
Copper 0.50 max.
Other 0.50 max.
Tungsten 0.50 max.
Silicon 0.08 max.
Phosphorus 0.04 max.
Sulfur 0.03 max.
Carbon 0.015 max.

Minimal Mechanical Properties:

Tensile (psi) 100,000
Mpa 690
Elongation (%) -

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.