Product Description:
HAYNES® Waspaloy RTW™ filler metal is used for the gas tungsten arc and gas metal arc welding of Waspaloy alloy. The deposited weld metal has excellent strength in the 1000°F-1800°F temperature range. The alloy is most commonly used for critical gas alloy turbine engine components. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.
Specifications:
AMS 5828 UNS N07001
Composition:
| Nickel | Remainder |
| Chromium | 18.00-21.00 |
| Cobalt | 12.00-15.00 |
| Molybdenum | 3.50-5.00 |
| Titanium | 2.75-3.50 |
| Iron | 2.00 max. |
| Aluminum | 1.20-1.60 |
| Carbon | 0.02-0.10 |
| Copper | 0.10 max. |
| Manganese | 0.10 max. |
| Silicon | 0.10 max. |
| Zirconium | 0.04 max. |
| Boron | 0.003-0.010 |
| Phosphorus | 0.0010 max. |
| Sulfur | 0.010 max. |
Minimal Mechanical Properties:
| Tensile (psi) | - |
| Mpa | - |
| Elongation (%) | - |
Available Product Forms and Sizes:
| Diameter in | 0.030 | 0.031 | 0.035 | 0.039 | 0.045 | 0.047 | 0.062 | 0.078 | 0.093 | *0.125 | *0.156x | 0.187x |
| Diameter mm | 0.76 | 0.80 | 0.89 | 1.00 | 1.10 | 1.20 | 1.60 | 2.00 | 2.40 | *3.20 | *4.00x | *4.70x |
Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.
*Size not available in MIG spools.
˟Size not available on reels.
Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.