Product Description:
HAYNES® 230-W®RTW™ filler metal is used for the gas tungsten arc and gas metal arc welding of HAYNES® 230-W®alloy. The filler metal may also be used to weld UNS N06617. The deposited weld metal combines excellent high temperature strength and oxidation resistance with superior long-term stability and good fabricability. The RTW™ finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.
Specifications:
AWS A5.14 ERNiCrWMo-1 UNS N06231
ASME SFA-5.14 ERNiCrWMo-1
AMS 5839
Composition:
| Nickel | Remainder |
| Chromium | 20.0-24.0 |
| Tungsten | 13.0-15.0 |
| Cobalt | 5.0 max. |
| Iron | 3.0 max. |
| Molybdenum | 1.00-3.00 |
| Manganese | 0.30-1.00 |
| Silicon | 0.25-0.75 |
| Aluminum | 0.20-0.50 |
| Copper | 0.50 max. |
| Other | 0.50 max. |
| Carbon | 0.05-0.15 |
| Lanthanum | 0.050 max. |
| Phosphorous | 0.03 max. |
| Sulfur | 0.015 max. |
| Boron | 0.003 max. |
Minimal Mechanical Properties:
| Tensile (psi) | 110,000 |
| Mpa | 760 |
| Elongation (%) | - |
Available Product Forms and Sizes:
| Diameter in | 0.030 | 0.031 | 0.035 | 0.039 | 0.045 | 0.047 | 0.062 | 0.078 | 0.093 | *0.125 | *0.156x | 0.187x |
| Diameter mm | 0.76 | 0.80 | 0.89 | 1.00 | 1.10 | 1.20 | 1.60 | 2.00 | 2.40 | *3.20 | *4.00x | *4.70x |
Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.
*Size not available in MIG spools.
˟Size not available on reels.
Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.