HAYNES® Ti-3Al-2.5V alloy |
---|
HAYNES® Ti-3Al-2.5-V alloy was developed for aircraft hydraulic and fuel systems transmission lines, primarily because of its high strength-to-weight ratio. This ratio proves to be a major advantage when used for hydraulic tubing lines to provide required strength levels, but more importantly, reducing weight by as much as 43% when compared to stainless steel. |