Alloy | Density lb./in3 (g/cm3)
| Sheet, Plate & Strip
| Billet Rod/Bar
| Coated Electrodes
| Bare Welding Rods
| Seamless Pipe & Tube
| Welded Pipe & Tube
| Fittings | Forgings | DIN | TUV | Other |
---|
HASTELLOY®
B-3® alloy N10675
(W80675)
| 0.333 (9.22)
| SB 333/B 333 P=44
| SB 335/ B335 B 472 P=44
| SFA 5.11/ A 5.11 (ENiMo-10) DIN 2.4696 (EL-NiMo28Cr) F= 44
| SFA 5.14/ A 5.14 (ERNiMo-10) DIN 2.4695 (SG-NiMo30Cr) F= 44
| SB 622/B 622 P=44
| SB 619/B 619 SB 626/B 626 P=44
| SB 366/B366 SB 462/B 462 P=44
| SB 564/B 564 SB 462/B 462 P=44
| 17744 No. 2.4600 NiMo29Cr
| Werkstoffblatt 517 Kennblatt 7615 Kennblatt 7616 Kennblatt 7617
| - |
HASTELLOY®
C-4 alloy N06455
(W86455)
| 0.312 (8.64)
| SB 575/B 575 P=43
| SB 574/B 574 P=43
| SFA 5.11/
A 5.11 (ENiCRMo-7) DIN 2.4612 (EL-NiMo15Cr15Ti) F= 43
| SFA 5.14/ A 5.14 (ERNiCrMo-7) DIN 2.4611 (SG-NiMo16Cr16Ti) F= 43
| SB 622/B 622 P=43
| SB 619/B 619 SB 626/B 626 P=43
| SB 366/B366 P=43
| | 17744 No. 2.4610 NiMo16Cr16Ti
| Werkstoffblatt 424 Kennblatt 2666 Kennblatt 2667 Kennblatt 2665
| NACE MR0175 ISO 15156
|
HASTELLOY®
C-22® alloy N06022
(W86022)
| 0.314 (8.69)
| SB 575/B 575 P=43
| SB 574/B 574 B 472 P=43
| SFA 5.11/ A 5.11 (ENiCrMo-10) DIN 2.4638 (EL-NiCr21Mo14W) F= 43
| SFA 5.14/ A 5.14 (ERNiCrMo-10) DIN 2.4635 (SG-NiCr21Mo14W) F= 43
| SB 622/B 622 P=43
| SB 619/B 619 SB 626/B 626 P=43
| SB 366/B366 SB 462/B 462 P=43
| SB 564/B 564 SB 462/B 462 P=43
| 17744 No. 2.4602 NiCr21Mo14W
| Werkstoffblatt 479 Kennblatt 4635 Kennblatt 4636 Kennblatt 4534
| NACE MR0175 ISO 15156 ASME Code Case No. 2226-2 Case No. N-621-1
|
HASTELLOY®
C-22HS® alloy N07022
| 0.311 (8.61)
| - | B 637 | - | - | B 983 | - | - | B 637 | - | - | NACE MR0175 |
HASTELLOY®
C-276 alloy N10276
(W10276)
| 0.321 (8.89)
| SB 575/B 575 P=43
| SB 574/B 574 B 472 P=43
| SFA 5.11/ A 5.11 (ENiCrMo-4) DIN 2.4887 (EL-NiMo15Cr15W) F= 43
| SFA 5.14/ A 5.14 (ERNiCrMo-4) DIN 2.4886 (SG-NiMo16Cr16W) F= 43
| SB 622/B 622 B 983 P=43
| SB 619/B 619 SB 626/B 626 P=43
| SB 366/B366 SB 462/B 462 P=43
| SB 564/B 564 SB 462/B 462 P=43
| 17744 No. 2.4819 NiMo16Cr15W
| Werkstoffblatt 400 Kennblatt 320 Kennblatt 319
| NACE MR0175 ISO 15156
|
HASTELLOY®
C-2000® alloy N06200 (W86200)
| 0.307 (8.58)
| SB 575/B 575 P=43
| SB 574/B 574 B 472 P=43
| SFA 5.11/ A 5.11 (ENiCrMo-17) DIN 2.4699 (EL-NiCr23Mo16Cu) F= 43
| SFA 5.14/ A 5.14 (ERNiCrMo-17) DIN 2.4698 (SG-NiCr23Mo16Cu) F= 43
| SB 622/B 622 P=43
| SB 619/B 619 SB 626/B 626 P=43
| SB 366/B366 SB 462/B 462 P=43
| SB 564/B 564 SB 462/B 462 P=43
| 17744 No. 2.4675 NiCr23Mo16Cu
| Werkstoffblatt 539 Kennblatt 9679 Kennblatt 9678 Kennblatt 9677
| NACE MR0175 ISO 15156
|
HASTELLOY®
G-30® alloy N06030
(W86030)
| 0.297 (8.22)
| SB 582/B 582 P=45
| SB 581/B 581 B 472 P=45
| SFA 5.11/ A 5.11 (ENiCrMo-11) F= 45
| SFA 5.14/ A 5.14 (ERNiCrMo-11) F= 45
| SB 622/B 622 P=45
| SB 619/B 619 SB 626/B 626 P=45
| SB 366/B366 SB 462/B 462 P=45
| SB 462/B 462 P=45
| No. 2.4603 NiCr30FeMo
| - | NACE MR0175 ISO 15156
|
HASTELLOY®
G-35® alloy N06035
| 0.297 (8.22)
| SB 575/B 575 P=43
| SB 574/B 574 B 472 P=43
| SFA 5.11/ A 5.11 (ENiCrMo-22) F= 43
| SFA 5.14/ A 5.14 (ERNiCrMo-22) F= 43
| SB 622/B 622 P=43
| SB 619/B 619 SB 626/B 626 P=43
| SB 366/B366 SB 462/B 462 P=43
| SB 564/B 564 SB 462/B 462 P=43
| No. 2.4643 NiCr33Mo8
| - | NACE MR0175 ISO 15156
|
HASTELLOY®
HYBRID-BC1® alloy
N10362
| 0.319 (8.83)
| B 575 P=43
| B 574 B 472 P=43
| - | ASME Cold Case No. 2653
| B622 P=43
| B 619 B 626 P=43
| B 366 P=43
| B 462 B 564 P=43
| No. 2.4708 NiMo22Cr15
| - | NACE MR0175 ISO 15156
|
HASTELLOY® N alloy N10003
| 0.320 (8.86)
| AMS 5607 SB 434/B 434 P=44
| AMS 5771 SB 573/B 573 P=44
| - | SFA 5.14/ A 5.14 (ERNiCrMo-2) F= 43
| - | - | SB 366/B366 P=44
| AMS 5771 | - | - | Mil-N24390B |
ULTIMET® alloy R31233
| 0.306 (8.47)
| SB 818/B 818 | B 815 | - | - | - | - | - | - | No. 2.4681 CoCr26Ni9Mo5W
| - | NACE MR0175/MR0103 ISO 15156
|