Form
|
Thickness/Diameter
|
Test Temperature
|
Impact Strength
|
Number
of Tests
|
-
|
in
|
mm
|
°F
|
°C
|
ft.lbf
|
J
|
-
|
Plate |
0.79 |
20 |
RT |
RT |
353 |
479 |
3 |
Plate |
0.79 |
20 |
-320 |
-196 |
334 |
453 |
3 |
Plate |
1.38 |
35 |
RT |
RT |
388 |
526 |
3 |
Plate |
1.38 |
35 |
-320 |
-196 |
359 |
487 |
3 |
Bar |
1.58 |
40 |
RT |
RT |
388 |
526 |
3 |
Bar |
1.58 |
40 |
-320 |
-196 |
339 |
460 |
3 |
Bar |
1.97 |
50 |
RT |
RT |
390 |
529 |
3 |
Bar |
1.97 |
50 |
-320 |
-196 |
338 |
458 |
3 |
*Charpy V-Notch Samples.
RT= Room Temperature