Product Description:

MULTIMET® RTW™ filler metal is used for the gas tungsten arc and gas metal arc welding of MULTIMET® alloy. The deposited weld metal has excellent strength at temperatures up to 1500°F and moderate strength up to 2000°F. The weld metal also has excellent oxidation resistance and good ductility. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AMS 5794   UNS R30155

Composition:

Iron: Remainder
Chromium: 20.0-22.50
Nickel: 19.0-21.0
Cobalt: 18.5-21.0
Molybdenum: 2.5-3.5
Tungsten: 2.0-3.0
Manganese: 1.0-2.0


 

Niobium: 0.75-1.25
Silicon: 1.0 max.
Nitrogen: 0.10-0.20
Carbon: 0.10 max.
Tantalum: 0.05 max.
Phosphorus: 0.04 max.
Sulfur: 0.03 max.


Minimal Mechanical Properties:

Tensile (psi) -
Mpa -
Elongation (%) -

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.