The Home of HASTELLOY® and
HAYNES® Alloys

HAYNES® Waspaloy RTW™ Filler Metal

Product Description:

HAYNES® Waspaloy RTW™ filler metal is used for the gas tungsten arc and gas metal arc welding of Waspaloy alloy. The deposited weld metal has excellent strength in the 1000°F-1800°F temperature range. The alloy is most commonly used for critical gas alloy turbine engine components. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AMS 5828    UNS N07001

Composition:

Nickel: Remainder
Chromium: 18.00-21.00
Cobalt: 12.00-15.00
Molybdenum: 3.50-5.00
Titanium: 2.75-3.50
Iron: 2.00 max.
Aluminum: 1.20-1.60

 

Carbon: 0.02-0.10
Copper: 0.10 max.
Manganese: 0.10 max.
Silicon: 0.10 max.
Zirconium: 0.04 max.
Boron: 0.003-0.010
Phosphorus: 0.0010 max.

 

Sulfur: 0.010 max.

Minimal Mechanical Properties:

Tensile (psi) -
Mpa -
Elongation (%) -

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.