phone-icon800.354.0806
765.456.6012
The Home of HASTELLOY® and
HAYNES® Alloys
Plasma Cutting

Tolerance Guidelines:
Material tolerances not listed below shall be in accordance with the ASTM, ASME, or AMS specification to which the material was produced and certified.

Southern Service Center (USA)

Thickness:     
Bed size:    
Minimum width/length:.
Minimum cut shape size:
Minimum hole size:
Kerf:

0.187” to 1.50”
110" x 300”
2× thickness with a minimum of 1”.
2× thickness with a minimum of 1”.
2× thickness with a minimum of 1”.
Approximately 0.50”

Standard plasma cutting tolerances that apply to both the top and bottom surfaces are as follows:

  • Up to 0.250 thick: + 0.125", -0        OD/ID + 0.125”/-0 OD & +0/-0.125” ID
  • .250" to 1.00" thick: + 0.1875", -0   OD/ID + 0.1875”/-0 OD & +0/-0.1875” ID
  • >1.00” thick: + 0.250", -0                OD/ID + 0.250”/-0 OD & +0/-0.250” ID
  • Diagonal tolerance: 3/16" maximum on plasma cut items.
  • Over 1.50" thick will be waterjet cut at outside source; please refer to waterjet tolerances.

If you require tighter tolerances, please contact one of our sales representatives.