Specifications for Corrosion-resistant Alloys
Alloy |
Densitylb./in3 (g/cm3) |
Sheet, Plate & Strip | BilletRod/Bar | Coated Electrodes | Bare Welding Rods | Seamless Pipe & Tube | Welded Pipe & Tube | Fittings | Forgings | DIN | TUV | Other |
HASTELLOY® B-3® alloy N10675 (W80675) | 0.333(9.22) | SB 333/B333 P=44 |
SB 335/ B335 |
SFA 5.11/ A 5.11(ENiMo-10) |
SFA 5.14/ A 5.14 |
SB 622/B 622 P=44 | SB 619/B619 SB 626/B 626 P=44 | SB 366/B366 SB 462/B 462 P=44 | SB 564/B564 SB 462/B 462 P=44 | 17744 No. 2.4600 NiMo29Cr | Werkstoffblatt 517 Kennblatt 7615 Kennblatt 7616 Kennblatt 7617 | – |
HASTELLOY® C-4 alloyN06455 (W86455) | 0.312(8.64) | SB 575/B 575 P=43 | SB 574/B 574 P=43 |
SFA 5.11/ A 5.11(ENiCRMo-7)DIN 2.4612 (EL-NiMo15Cr15Ti) F= 43 |
SFA 5.14/ A 5.14(ERNiCrMo-7) DIN 2.4611 (SG-NiMo16Cr16Ti) F= 43 |
SB 622/B 622 P=43 | SB 619/B619 SB 626/B 626 P=43 | SB 366/B366 P=43 | - | 17744 No. 2.4610 NiMo16Cr16Ti | Werkstoffblatt 424 Kennblatt 2666 Kennblatt 2667 Kennblatt 2665 | NACE MR0175 ISO 15156 |
HASTELLOY® C-22® alloy N06022 (W86022) | 0.314(8.69) | SB 575/B 575 P=43 | SB 574/B574 B 472 P=43 |
SFA 5.11/ A 5.11(ENiCrMo-10) DIN 2.4638 (EL-NiCr21Mo14W) F= 43 |
SFA 5.14/ A 5.14(ERNiCrMo-10) DIN 2.4635 (SG-NiCr21Mo14W) F= 43 |
SB 622/B 622 P=43 | SB 619/B619 SB 626/B 626 P=43 | SB 366/B366SB 462/B 462 P=43 | SB 564/B564 SB 462/B 462 P=43 | 17744 No. 2.4602 NiCr21Mo14W | Werkstoffblatt 479 Kennblatt 4635 Kennblatt 4636 Kennblatt 4534 | NACE MR0175 ISO 15156 ASME Code Case No. 2226-2Case No. N-621-1 |
HASTELLOY®C-22HS® alloy N07022 | 0.311(8.61) | – | B 637 | – | – | B 983 | – | – | B 637 | – | – | NACE MR0175 |
HASTELLOY® C-276 alloy N10276 (W10276) | 0.321(8.89) | SB 575/B 575 P=43 | SB 574/B574 B 472 P=43 |
SFA 5.11/ A 5.11(ENiCrMo-4) DIN 2.4887 (EL-NiMo15Cr15W) F= 43 |
SFA 5.14/ A 5.14(ERNiCrMo-4)DIN 2.4886 (SG-NiMo16Cr16W) F= 43 |
SB 622/B 622B 983 P=43 | SB 619/B619 SB 626/B 626 P=43 | SB 366/B366 SB 462/B462 P=43 | SB 564/B564 SB 462/B 462 P=43 | 17744 No. 2.4819 NiMo16Cr15W | Werkstoffblatt 400 Kennblatt 320 Kennblatt 319 | NACE MR0175 ISO 15156 |
HASTELLOY®C-2000® alloy N06200 (W86200) | 0.307(8.58) | SB 575/B 575 P=43 | SB 574/B574 B 472 P=43 |
SFA 5.11/ A 5.11(ENiCrMo-17) DIN 2.4699 (EL-NiCr23Mo16Cu) F= 43 |
SFA 5.14/ A 5.14(ERNiCrMo-17)DIN 2.4698(SG-NiCr23Mo16Cu) F= 43 |
SB 622/B 622 P=43 | SB 619/B619 SB 626/B 626 P=43 | SB 366/B366 SB 462/B462 P=43 | SB 564/B564 SB 462/B 462 P=43 | 17744 No. 2.4675NiCr23Mo16Cu | Werkstoffblatt 539 Kennblatt 9679 Kennblatt 9678 Kennblatt 9677 | NACE MR0175 ISO 15156 |
HASTELLOY® G-30® alloy N06030 (W86030) | 0.297(8.22) | SB 582/B 582 P=45 | SB 581/B 581B 472 P=45 |
SFA 5.11/ A 5.11(ENiCrMo-11) F= 45 |
SFA 5.14/ A 5.14(ERNiCrMo-11) F= 45 |
SB 622/B 622 P=45 | SB 619/B619 SB 626/B 626 P=45 | SB 366/B366 SB 462/B 462 P=45 | SB 462/B 462 P=45 | No. 2.4603 NiCr30FeMo | – | NACE MR0175 ISO 15156 |
HASTELLOY® G-35® alloy N06035 | 0.297(8.22) | SB 575/B 575 P=43 | SB 574/B 574B 472 P=43 |
SFA 5.11/ A 5.11(ENiCrMo-22) F=43 |
SFA 5.14/ A 5.14 (ERNiCrMo-22) F=43 |
SB 622/B 622 P=43 | SB 619/B619 SB 626/B 626 P=43 | SB 366/B366 SB 462/B 462 P=43 | SB 564/B564 SB 462/B 462 P=43 | No. 2.4643 NiCr33Mo8 | – | NACE MR0175 ISO 15156 |
HASTELLOY® HYBRID-BC1® alloy N10362 | 0.319(8.83) | B 575 P=43 | B 574 B 472 P=43 | – | ASME Code Case No. 2653 | B622 P=43 | B 619 B 626 P=43 | B 366 P=43 | B 462B 564 P=43 | No. 2.4708 NiMo22Cr15 | – | NACE MR0175 ISO 15156 |
HASTELLOY® N alloy N10003 | 0.320(8.86) | AMS 5607 SB 434/B 434 P=44 | AMS 5771 SB 573/B 573 P=44 | – |
SFA 5.14/ A 5.14 (ERNiCrMo-2) F= 43 |
– | – | SB 366/B366 P=44 | AMS 5771 | – | – | Mil-N24390B |
ULTIMET® alloy R31233 | 0.306(8.47) | SB 818/B 818 | SB 815/B 815 | – | – | – | – | – | – | No. 2.4681 CoCr26Ni9Mo5W | – | NACE MR0175/MR0103 ISO 15156 |