  • へインズインターナショナル社がHAYNES® 244® 合金の開発を発表。

    Haynes International, Inc. is pleased to announce the development of HAYNES® 244® alloy. This alloy has an excellent combination of high temperature strength, low thermal expansion behavior, thermal stability, and good oxidation resistance at temperatures up to 1400°F (760°C).