Thermal Spray 

Alloy UNS Specifications
AWS/ASME AMS
HAYNES® 20CB-3
N08021 ER320/320LR  -
HAYNES® 72 N06072 ERNiCr-4  -
HAYNES® 80/20 N06003  - ASTM B344
HAYNES® 95/5 N03301  -  -
HAYNES® 200
N02200 ERNi-C1, UNS N02215 ASTM B160
HAYNES® 202 S20200 W-FeCrNi-3, UNS S20281  -
HAYNES® 316L S31603  - ASTM A580
HAYNES® 420 S42000 ER420  -
HAYNES® 625 N00625 ERNiCrMo-3 AMS 5837
HAYNES® C-276 N10276 ERNiCrMo-4  -