HASTELLOY®およびHAYNES® 合金のホームページ

Coated Electrodes

Corrosion-resistant Alloys
Coated Electrodes* Specifications
Alloy UNS AWS/ASME AMS Other
HASTELLOY® B-3®
W80675 ENiMo-10  -
HASTELLOY® C-4
W86455 ENicRMo-7  -
HAYNES® C-22®/122
W86022 ENiCrMo-10  -
HASTELLOY® C-276
W80276 ENiCrMo-4  -
HASTELLOY® C-2000
W86200 ENiCrMo-17  -
HASTELLOY® G-30®
W86030 ENiCrMo-11  -
HASTELLOY® G-35®
W86035 ENiCrMo-22  -
ULTIMET®
R31233  -  -
High-temperature Alloys
Coated Electrodes* Specifications
Alloy UNS AWS/ASME AMS Other
HAYNES® 112  W86112  ENiCrMo-3  -  625 Core
HAYNES® 117  W86117  ENiCrCoMo-1  -  617 Core
HAYNES® 182  W86182  ENiCrFe-3  -
MULTIMET®  W73155  E3155  AMS 5795 
HAYNES® 230-W  W86231  ENiCrWMo-1  - -
HASTELLOY® X
W86002 ENiCrMo-2  -

*Other alloys available upon request.
For individual coated electrode data sheets, please click on the alloy.