Corrosion-resistant Alloys

Specifications Available Forms
Alloy UNS Seamless
Pipe & Tubing
Welded
Pipe & Tubing
Tubing Pipe
Welded Seamless Welded Seamless
B-3® N10675 SB 622/B 622 SB 619/B 619
SB 626/B 626
available forms available forms available forms available forms 
C-4 N06455 SB 622/B 622 SB 619/B 619
SB 626/B 626
available forms available forms available forms available forms
C-22® N06022 SB 622/ B 622 SB 619/B 619
SB 626/B 626
available forms available forms available forms available forms
C-22HS® N07022 B 983 - available with approval available with approval oil available with approval available with approval oil
C-276® N10276 SB 622/B 622 SB 619/B 619
SB 626/B 626
available forms available forms oil available forms available forms oil
C-2000® N06200 SB 622/B 622 SB 619/B 619
SB 626/B 626
available forms available forms available forms available forms
G-30® N06030 SB 622/B 622 SB 619/B 619
SB 626/B 626
available forms available forms available forms available forms
HYBRID-BC1® N10362 B 622 B 619
B 626
available with approval available with approval available with approval available with approval

available forms Available from stock in select sizes available with approval Available with approval and minimum quantities   oilOil country tubulars