Haynes to Present at NACE Conference & Corrosion Expo

by Kierstin Bott | Mar 16, 2018

Please join our alloy experts as they present their technical papers during the NACE Conference & Corrosion Expo, April 16th and 18th in Phoenix, AZ.

Monday, April 16th
1:50pm Room: 228 A-B

Picture2

Presenter: Ajit Mishra Session Information: Mechanisms of Localized Corrosion and Electrochemical Methods Presentation Title: “Role of Major and Minor Alloying Elements in CRAs toLocalized Corrosion Inhibition: A Review ”

 

Wednesday, April 18th
8:35am 
Room: 222 B-C

Picture2

Presenter: Ajit Mishra
Session Information: Recent Experiences with Nickel, Titanium, Zirconium and Other Corrosion Resistance Alloys 
Presentation Title: “Sensitization Study of Corrosion-Resistant Nickel-Alloys”

 

9:00am Room: 222 B-C

Picture1Presenter: Jeremy Caron
Session Information: Recent Experiences with Nickel, Titanium, Zirconium and Other Corrosion Resistance Alloys
Presentation Title: “Welding Metallurgy and Weld Metal Properties of UNS N07022 Alloy”