MULTIMET® Coated Electrodes

Product Description:

MULTIMET® coated electrodes are used for the shielded metal arc welding of HAYNES® HR-120® alloy. The electrodes are also a great candidate for dissimilar joining of other high-temperature materials including HAYNES® 556® alloy, HAYNES® HR-160® alloy and other nickel and cobalt high-temperature alloys. The coating is designed for great operability, especially in out-of-position welding.

Specifications:

AMS 5795 

Composition:

Iron: Remainder
Chromium: 20.0-22.5
Nickel: 19.0-21.0
Cobalt: 18.5-21.0
Molybdenum: 2.5-3.5
Tungsten: 2.0-3.0

Manganese: 1.0-2.5
Niobium + Tantalum 0.75-1.25
Silicon: 1.0 max.
Carbon: 0.10 max.
Phosphorus: 0.04 max.
Sulfur: 0.03 max.

Minimal Mechanical Properties:

Tensile (psi) 90,000
Mpa 620
Elongation (%) 20

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150