Product Description:

HAYNES® 230-W® coated electrodes are used for the shielded metal arc welding of HAYNES® 230®. The deposited weld metal has excellent high-temperature strength and outstanding resistance to oxidizing environments up to 2100°F for prolonged exposures. The deposited weld metal also has excellent long-term stability.

Specifications:

AWS A 5.11 ENiCrWMo-1     UNS W86231

Composition:

Nickel: Remainder
Chromium: 20.00-24.00
Tungsten: 13.00-15.00
Cobalt: 5.00 max.
Iron: 3.00
Molybdenum: 1.00-3.00
Manganese: 0.30-1.00

 

Silicon: 0.25-0.75
Other: 0.50 max.
Copper: 0.50 max.
Aluminum: 0.50 max.
Titanium: 0.10 max.
Carbon: 0.10 max.
Phosphorus: 0.02 max.

 

Sulfur: 0.0015

Minimal Mechanical Properties:

Tensile (psi) 90,000
Mpa 620
Elongation (%) 20

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150