HASTELLOY® G-35® Coated Electrodes

Product Description:

HASTELLOY® G-35® coated electrodes are used for the shielded metal arc welding of G-35® alloy. The deposited weld metal has outstanding corrosion resistance to “fertilizer-grade” phosphoric acid, other oxidizing acids, alkalis, and chloride-bearing media. The electrodes can also be used for the overlay and cladding of carbon steels where enhanced corrosion resistance is needed.

Specifications:

AWS A 5.11 ENiCrMo-22     UNS W86035

Composition:

Nickel: Balance
Chromium: 32.25-34.25
Molybdenum: 7.6-9.0
Iron: 2.0 max.
Cobalt: 1.0 max.
Manganese: 0.5 max.
Silicon: 0.6 max.

 

Carbon: 0.05 max.
Copper: 0.3 max.
Niobium + Tantalum 0.50 max.
Tungsten: 0.60 max.
Aluminum: 0.40 max.
Titanium: 0.20 max.
Vanadium: 0.20 max.

 

Phosphorus: 0.03 max.
Sulfur: 0.015 max.
Other: 0.50 max.

Minimum Mechanical Properties:

Tensile (psi) 85,000
Mpa 590
Elongation (%) 25

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150