Standard Sizes

Welding Consumables
Loose Coil Diameters Precision Layer Wound RTW™ Wire Diameters Cut Lengths (GTAW)* Diameters Drum Pack Diameters  Coated Electrodes Diameters
in mm in mm in mm in  mm in mm
0.030 0.76 0.030 0.76 0.030 0.76 0.045  1.10  0.093 2.40
0.031 0.80 0.031 0.79 0.031 0.79 0.062  1.60  0.125 3.20
0.035 0.89 0.034 0.89 0.035 0.89 0.125  3.20  0.156 4.00
0.039 1.00 0.039 1.00 0.039 1.00   0.187 4.70
0.045 1.10 0.045 1.10 0.045 1.10  
0.062 1.60 0.062 1.60 0.062 1.60
0.078 2.00 0.078 2.00 0.078 2.00
0.093 2.40 0.093 2.40 0.093 2.40
0.125 3.20 0.125  3.20  0.125 3.20
0.156 4.00   0.156 4.00
0.187 4.70 0.187 4.70

*Other sizes available upon request

Wire Rod
Wire Rod for Redraw
in mm
0.218 5.50
0.250 6.40
0.256 6.50
0.275 7.00
HRAP (Hot Rolled, Annealed & Pickled)

*Other sizes available upon request

Small Bar
Coil and Cut Length
Diameters
in mm
0.187 4.70
0.250 6.40
0.312 7.90
0.375 9.50
 0.500 12.70
 0.625  15.90
 0.750  19.00
(As Cold Drawn, Solution Heat-treated, or Solution Heat-treated & Ground)

*Other sizes available upon request