Specifications and Codes

Specifications

Codes

HAYNES® X-750 alloy
(N07750)
Sheet, Plate & Strip AMS 5542
AMS 5598
Billet, Rod & Bar AMS 5667
AMS 5668
AMS 5670
AMS 5671
AMS 5747
Coated Electrodes -
Bare Welding Rods & Wire AMS 5778
SFA 5.14/ A 5.14 (ERNiCrFe-8)
Seamless Pipe & Tube -
Welded Pipe & Tube -
Fittings -
Forgings AMS 5667
AMS 5668
AMS 5670
AMS 5671
AMS 5747
SB 637/B 637
DIN No. 2.4669
NiCr15Fe7TiAl
Others NACE MR0175
ISO 15156
HAYNES® X-750 alloy
(N07750)
MMPDS  6.3.6