phone-icon800.354.0806
765.456.6012
The Home of HASTELLOY® and
HAYNES® Alloys

Aged Hardness

Age Hardened Room Temperature Hardness

Form Hardness Heat Treatment
Sheet 35 HRC 2050F, 30 Min, AC + 1650F, 4 Hr, AC
Plate 36 HRC 2050F, 30 Min, AC + 1650F, 4 Hr, AC
Sheet 42 HRC 1400F, 16 Hr, AC
Plate 39 HRC 1400F, 16 Hr, AC

HRC = Hardness Rockwell "C"