Specifications

HAYNES® 617 (N06617)
Products
ASTM ASME Section II AMS Other
Sheet, Plate & Strip B168 SB-168 5888
5889
-
Billet, Rod & Bar B166
B472
SB-166 5887 -
Seamless Pipe B167 SB-167 - -
Welded Pipe B546 - - -
Seamless Tube B167 SB-167 - -
Welded Tube B626 - - -
Fittings - - - -
Forgings B564 SB-564 - -
Weld Consumables (W86117)
AWS ASME Section II* AMS Other
Coated Electrodes
(Classification)
A5.11
(ENiCrCoMo-1)
SFA 5.11
(ENiCrCoMo-1)
- -
Bare Welding Rods & Wire
(Classification)
A5.14
(ERNiCrCoMo-1)
SFA 5.14
(ERNiCrCoMo-1)
- -

*The associated ASME Section IX P No. for welding is 43; the P No. for brazing is 111.

Codes

 HAYNES® 617 Alloy (N06617, W86117)
Max Design Temperatures
ASME BPV Section I 1650°F (899°C)1,2,3
Section III, Class 1 -
Section III, Class 2 -
Section III, Class 3 -
Section IV -
Section VIII, Div. 1 1800°F (982°C)1,2,4
Section VIII, Div. 2 -
Section VIII, Div. 3 -
Section XII -
B16.5 -
B16.34 -
B31.1 1200°F (649°C)1,5
B31.3 -
MMPDS - -
  1. Approved forms are Plate, Sheet, Strip, Bar/Rod, Forgings, Seamless Pipe/Tube
  2. Welded Tube is currently permitted per BPV I Code Case 2923
  3. Additional BPV I Code Cases govern usage:
  4.     a. Code Case 2439 permits water wetted service usage up to 1200°F (649°C)
        b. Weld Strength Reduction Factors are governed by Code Case 2805
  5. Weld Strength Reduction Factors are governed by Code Case 2805
  6. This alloy is permitted for bolting per BPV VIII, Div. 1 Code Case 2776
  7. Seamless Pipe/Tube and Forgings are permitted per B31 Case 203 for water wetted Boiler External Piping (BEP) up to 1250°F (677°C).