Specifications

Codes

HAYNES® HR-120® alloy
(N08120)
Sheet, Plate & Strip AMS 5916
SB 409/B 409
P= 45
Billet, Rod & Bar SB 408/B 408
B 472
P= 45
Coated Electrodes -
Bare Welding Rods & Wire -
Seamless Pipe & Tube SB 407/B 407
SB 163/B 163
P= 45
Welded Pipe & Tube SB 514/B 514
SB 515/B 515
P= 45
Fittings SB 366/B 366
P= 45
Forgings SB 564/B 564
P= 45
DIN No. 2.4854
NiFe33Cr25Co
Others -
HAYNES® HR-120® alloy
(N08120)
ASME Section l -
Section lll Class 1 -
Class 2 -
Class 3 -
Section lV HF-300.2 -
Section Vlll Div. 1 1800°F (982°C)1,2
Div. 2 -
Section Xll -
B16.5 -
B16.34 -
B31.1 -
B31.3 -
MMPDS 6.3.10
1Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube
2Properties up to 1650ºF (899ºC) are found in the latest ASME BPV Code, and from 1650ºF - 1800ºF (899ºC - 982ºC) in ASME Code Case 2672