HASTELLOY® N alloy
(N10003)
Sheet, Plate & Strip AMS 5607
SB 434/B 434
P= 44
Billet, Rod & Bar AMS 5771
SB 573/B 573
P= 44
Coated Electrodes -
Bare Welding Rods & Wire SFA 5.14/ A 5.14 (ERNiMo-2)
F= 44
Seamless Pipe & Tube -
Welded Pipe & Tube -
Fittings SB 366/B 366
P= 44
Forgings AMS 5771
DIN -
TÜV -
Others Mil-N24390B
HASTELLOY® N alloy
(N10003)
ASME Section l -
Section lll Class 1 -
Class 2 -
Class 3 -
Section Vlll Div. 1 1300°F (704°C)1
Div. 2 800°F (427°C)1
Section Xll 650°F (343°C)1
B16.5 1300°F (704°C)2
B16.34 1300°F (704°C)2
B31.1 -
B31.3 -
VdTÜV (doc #) -
1Plate, Sheet, Bar
2Plate, Bar