High-Cycle Fatigue

Material: 0.5 in Diameter 43% Cold Worked Bar (0.2%YS – 191 ksi, UTS – 196 ksi, %EL – 18, %RA – 66)
Rotating Bend Fatigue Testing, RR Moore Rotating 4-Point Bend
R = -1.0 Stress Ratio, 167 Hz, Room Temperature

C-22HS cycle fatigue