phone-icon800.354.0806
765.456.6012
The Home of HASTELLOY® and
HAYNES® Alloys

Specifications and Codes

Specifications

Codes

HASTELLOY® C-4 alloy
(N06455, W86445)
Sheet, Plate & Strip SB 575/B 575
P= 43
Billet,  Rod & Bar SB 574/B 574
P= 43
Coated Electrodes SFA 5.11/ A 5.11 (ENiCrMo-7)
F=43
Bare Welding Rods & Wire SFA 5.14/ A 5.14 (ERNiCrMo-7)
F= 43
Seamless Pipe & Tube SB 622/B 622
P= 43
Welded Pipe & Tube SB 619/B 619
P= 43
Fittings SB 366/B 366
P= 43
Forgings -
DIN 17744 No. 2.4610 NiMo16Cr16Ti
TÜV Werkstoffblatt 424
Kennblatt 2666.02
Kennblatt 2667.02
Kennblatt 2665.02
Others NACE
HASTELLOY® C-4 alloy
(N06455, W86455)
ASME Section l -
Section lll Class 1 -
Class 2 -
Class 3 -
Section Vlll Div. 1 800°F (427°C)1
Div. 2 800°F (427°C)2
Section Xll 650°F (343°C)1
B16.5 800°F (427°C)3
B16.34 800ºF (427°C)4
B31.1 -
B31.3 800°F (427°C)1
VdTÜV (doc #) 752°F (400ºC) 5,
#424
1Plate, Sheet, Bar, fittings, welded pipe/tube, seamless pipe/tube
2Plate, Sheet, Bar, welded pipe/tube, seamless pipe/tube
3Plate, Forgings, fittings
4Plate, Bar, Forgings, seamless pipe/tube
5Plate, Sheet, Bar, Forgings, seamless pipe/tube
Print Page