Specifications and Codes

Specifications

Codes

HASTELLOY® B-3® alloy
(N10675, W80675)
Sheet, Plate & Strip SB 333/B 333
P= 44
Billet, Rod & Bar SB 335/B 335
B 472
P= 44
Coated Electrodes SFA 5.11/ A5.11 (ENiMo-10)
F= 44
Bare Welding Rods & Wire SFA 5.14/ A5.14 (ERNiMo-10)
F= 44
Seamless Pipe & Tube SB 622/B 622
P= 44
Welded Pipe & Tube SB 619/B 619
P= 44
Fittings SB 366/B 366
P= 44
Forgings SB 564/B 564
P= 44
DIN 17744 No. 2.4600 NiMo29Cr
TÜV Werkstoffblatt 517
Kennblatt 7615.00
Kennblatt 7616.00
Kennblatt 7617.00
Others -
HASTELLOY® B-3® alloy
(N10675, W80675)
ASME Section l -
Section lll Class 1 -
Class 2 -
Class 3 800ºF (427ºC)1
Section Vlll Div. 1 800ºF (427ºC)1
Div. 2 -
Section Xll 650°F (343°C)2
B16.5 800°F (427°C)3
B16.34 800°F (427°C)4
B31.1 -
B31.3 800°F (427°C)5
VdTÜV (doc #) 752°F (400ºC)6
#517
1Plate, Sheet, Bar, Forgings, welded pipe/tube, seamless pipe/tube
2Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube
3Plate, Forgings, fittings
4Plate, Bar, Forgings, seamless pipe/tube
5Plate, Sheet, Bar, fittings, welded pipe/tube, seamless pipe/tube
6Plate, Sheet, Bar, Forgings